Materials / Mechanical Engineering
Hardness Conversion Calculator
Convert approximate hardness values between Rockwell C, Rockwell B, Vickers and Brinell scales for non-austenitic steels.
Converted hardness values are approximate equivalents, not substitute test results.
Hardness scales do not have a universal one-to-one physical conversion. Scope: homogeneous non-austenitic carbon, alloy and tool steels. Verify suitability for the actual material and heat treatment.
Measured hardness
Material scope: Non-austenitic carbon/alloy/tool steels
Supported input range: 20.168167–67.814613 HRC
Approximate equivalents
Input: 40 HRC
- Vickers (HV)
391 HV
Approximate equivalent
- Brinell (HBW)
370 HBW
Approximate equivalent
- Rockwell C (HRC)
40.0 HRC
Same input scale
- Rockwell B (HRB)
—
Not available for this hardness range
Curves stop at the implemented domain limits. No extrapolation.
Why hardness conversion is approximate
Brinell and Vickers measure indentation size; Rockwell measures indentation depth. Different indenters and loads probe material response differently. Composition, microstructure, heat treatment, work hardening, testing method and surface condition affect the correlation. These are empirical equations, not physical unit conversions.
Vickers hardness
HV uses a diamond pyramid and the indentation diagonals. It covers a wide hardness range; this calculator uses HV as its internal axis. The implemented correlations do not establish validity for microhardness measurements of thin layers.
Brinell hardness
HBW uses a tungsten-carbide ball and indentation diameter, typically for bulk material testing. Here the published relationship is limited to a 10 mm ball and 3000 kgf load, 226–634 HBW. It must not be confused with legacy steel-ball HBS. No soft-steel HBW relationship is implemented.
Rockwell C
HRC uses a diamond cone and a 150 kgf total test force, commonly for harder steels. Only the implemented higher-HV branch is used; a numerical equation result below its domain is not reported.
Rockwell B
HRB uses a ball indenter and a 100 kgf total test force, commonly for softer metallic materials. This tool restricts the relationship to homogeneous non-austenitic steel and 100–240 HV; it does not extend to other metals.
Conversion method and sources
Equation-based implementation using the publicly documented correlations below, not a reproduction of standard conversion tables. HV is the common axis. Dependent scales are inverted by bracketed bisection (80 iterations); no anchor-point interpolation or extrapolation is used.
HRC(HV) = 31.49 + 0.0796683·HV − 3.55432×10⁻⁵·HV² − 6728.16/HV
HRB(HV) = 114.665 + 0.0882795·HV − 1.41855×10⁻⁴·HV² − 6695.28/HV
HRC(HBW) = 18.1673 + 0.120388·HBW − 6.94388×10⁻⁵·HBW² − 4883.27/HBW
Conservative source domains: HRC relation 238–940 HV; HRB relation 100–240 HV; HBW relation 226–634 HBW. Input HRC is 20.168166547…–67.814613459… and HRB is 55.1216–99.784232: equation images of those domains, not rounded standard-table endpoints. HV input is 100–940. Each output must satisfy its own domain; HBW stops at about 58.88 HRC. Both Rockwell branches are available in the 238–240 HV overlap.
Output rounding: HV/HBW to whole numbers; HRC/HRB to 0.1. Unrounded values drive domain checks. Tensile-strength estimation, HRA and HK are not implemented. Numerical solving precision is not empirical accuracy.
Recognized references such as ASTM E140 and ISO 18265 use material-specific approximate conversion principles. This implementation was checked against the publicly readable equations, not against a licensed current standard or specimen test data.